Effect of wide change of cooling rate on dendritic segregation of a directionally solidified cobalt-base superalloy
宽变冷速对定向凝固合金枝晶偏析的影响
Simultaneous multielement determination for superalloy by glow discharge optical emission spectrometry ( GDOES ) was investigated.
研究了用辉光光谱法 ( GDOES ) 同时测定高温合金中的多种元素的含量.
low cycle fatigue tests of a directionally solidified nickel base superalloy were conducted at elevated temperatures.
本文研究了一种定向凝固镍基高温合金的高温低周疲劳行为.